Volume 9, 1973, Issue 31
Modification and material change on Key West Desalting Plant
Thanks to hydrogen sulfide, corrosion attack on cu-ni tubes, trays, lining and monel demisters, the plant's heat exchangers had to be retubed with...
Thanks to hydrogen sulfide, corrosion attack on cu-ni tubes, trays, lining and monel demisters, the plant's heat exchangers had to be retubed with...